CAF 765

OVERVIEW: Heat resistant stainless steel alloy.

TYPICAL USES: Petrochemical parts.

MetalTek Grade: CAF 765

Typical Chemical Composition (% by wt.)

Cr: 25.0 - 27.5

Fe: Bal

Mn: 1.0 max

Ni: 34.0 - 36.5

Si: 1.4 - 2.0

W: 4.5 - 5.5

C Max: 0.45 - 0.50

Other: Co 14.0 - 16.0

Minimum Mechanical Properties

Tensile, ksi: 70

Tensile, MPa: 480

Yield, ksi: 40

Yield, MPa: 270

Elongation %: 4