CAF 769

OVERVIEW: Heat resistant stainless steel alloy.

TYPICAL USES: Petrochemical components.

MetalTek Grade: CAF 769

Typical Chemical Composition (% by wt.)

Cr: 25.0 - 28.0

Fe: Bal

Mn: 0.5 - 1.25

Ni: 35.0 - 38.0

Si: 0.8 - 1.5

W: 1.25 - 2.00

C Max: 0.40 - 0.50