Cast Grade: N-7M

OVERVIEW: Corrosion and heat resistant alloy.

MetalTek Grade: MTEK N-7M

Similar Specifications

Cast UNS: N30007

Cast Grade: N-7M

Cast ASTM: A494

Wrought UNS: N10001

Typical Chemical Composition (% by wt.)

Cr: 1.00

Fe: 3.0 MAX

Mn: 1.00

Ni: Bal

Si: 1.00

C Max: 0.07

Other: Mo 30-33

Minimum Mechanical Properties

Tensile, ksi: 76

Tensile, MPa: 525

Yield, ksi: 40

Yield, MPa: 275

Elongation %: 20

Heat Treatment: SOLUTION ANNEAL