Cast Grade: Alloy 713

OVERVIEW: This alloy is resistant to thermal fatigue and has excpetional rupture strength.

TYPICAL USES: Aerospace applications.

MetalTek Grade: IN® 713

Similar Specifications

Cast Grade: Alloy 713

Wrought UNS: N07713

Wrought Grade: IN® 713

Military / AMS: AMS 5377 (INVEST); AMS 5391 (INVEST)

Typical Chemical Composition (% by wt.)

Al: 5.50 - 6.50

Cr: 13 - 15

Ni: Bal

C Max: 0.20

Other: Mo 2.5 - 5.5; Ti 0.75 - 1.25; Nb (Cb) 4.75 - 5.40; Zr; Ta 1-3; B

Minimum Mechanical Properties

Tensile, ksi: 110

Tensile, MPa: 760

Yield, ksi: 100

Yield, MPa: 690

Elongation %: 3

Heat Treatment: As Cast