Alloy Grade UNS: HW – Excellent Carburization Resistance

  • Overview

    Not as strong as HT but high nickel content delivers excellent carburization resistance. Service limit  980 degree Celsius (1800 degrees Fahrenheit).

  • Typical Uses

    Cyanide pots, molten lead heating elements, retorts.

  • MetalTek Grade

    MTEK 10-60

Similar Specifications

Cast UNS: N08001

Cast Grade: HW

Cast ASTM: A297

Typical Chemical Composition (% by wt.)

Aluminum: n/a

Carbon: 0.35-0.75

Chromium: 10.0-14.0

Manganese: 2

Iron: n/a

Copper: n/a

Nickel: 58-62

Lead: n/a

Tin: n/a

Silicon: 2.5

Zinc: n/a

Minimum Mechanical Properties

Tensile, ksi

0

Tensile, MPa

0

Heat Treatment: Not Heat Treated